Grade C55E4
Corresponding Standard JIS G 7105-2000
Heat-Treatable Steels, Alloy Steels and Free-Cutting Steels — Part 18 : Bright Products Of Unalloyed and Low Alloy Steels
Classification Carbon Steel
Properties Carburizing Ability
C55E4 Chemical Element Composition Content (%)
Component C Si Mn P S
Minimum Value 0.52 0.1 0.6 - -
Maximum Value 0.6 0.4 0.9 0.035 0.035
◎ Steels with machinability which has been improved either by the addition of lead or by higher sulfur levels up to about 0.100 % (m/m) S (including controlled sulfide morphology) may be available on request.
C55E4 Mechanical Properties
thickness
t
mm
Heat Treatment or Condition
Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
Hardness
HBW
t≤5 TC ≥820 ≥670 ≥4
5<t≤10 TC ≥800 ≥620 ≥5
10<t≤16 TC ≥780 ≥590 ≥5
16<t≤25 TC ≥740 ≥535 ≥6
25<t≤40 TC ≥720 ≥510 ≥6
40<t≤100 TC ≥640 ≥330 ≥7
t≤100 TC+TA,
P+TA
or
G+TA
≥229
t≤16 TC+TN,
P+TN
or
G+TN
≥680 ≥370 ≥11
16<t≤100 TC+TN,
P+TN
or
G+TN
≥640 ≥330 ≥12
100<t≤250 TC+TN,
P+TN
or
G+TN
≥620 ≥300 ≥12
t≤16 TC+TQ+TT℗,
P+TQ+TT
or
G+TQ+TT
800~950 ≥550 ≥12
16<t≤40 TC+TQ+TT℗,
P+TQ+TT
or
G+TQ+TT
750~900 ≥490 ≥14
40<t≤100 TC+TQ+TT℗,
P+TQ+TT
or
G+TQ+TT
700~850 ≥420 ≥15
100<t≤250 TC Be agreed Be agreed Be agreed
100<t≤250 TC+TA,
P+TA
or
G+TA
Be agreed
100<t≤250 TC+TQ+TT,
P+TQ+TT
or
G+TQ+TT
Be agreed Be agreed Be agreed