Grade 28Mn6
Corresponding Standard JIS G 7105-2000
Heat-Treatable Steels, Alloy Steels and Free-Cutting Steels — Part 18 : Bright Products Of Unalloyed and Low Alloy Steels
Classification Alloy Steel
Properties Carburizing Ability
28Mn6 Chemical Element Composition Content (%)
Component C Si Mn P S
Minimum Value 0.25 0.1 1.3 - -
Maximum Value 0.32 0.4 1.65 0.035 0.035
◎ Steels with machinability which has been improved either by the addition of lead or by higher sulfur levels up to about 0.100 % (m/m) S (including controlled sulfide morphology) may be available on request.
28Mn6 Mechanical Properties
thickness
t
mm
Heat Treatment or Condition
Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
Hardness
HBW
Impact Energy Absorption
KV2
J
t≤16 TC ≤920
16<t≤40 TC ≤900
40<t≤80 TC ≤880
t≤80 TC+TA,
P+TA
or
G+TA
≤223
t≤16 TC+TQ+TT℗,
P+TQ+TT
or
G+TQ+TT
800~950 ≥590 ≥13 KU: ≥25
KV: ≥35
16<t≤40 TC+TQ+TT℗,
P+TQ+TT
or
G+TQ+TT
700~850 ≥490 ≥15 KU: ≥30
KV: ≥40
40<t≤80 TC+TQ+TT℗,
P+TQ+TT
or
G+TQ+TT
650~800 ≥440 ≥16 KU: ≥30
KV: ≥40