Grade A814 TP XM-15
USA UNS S38100
Corresponding Standard ASTM A814/A814M-2015(R2019)
Standard Specification for Cold-Worked Welded Austenitic Stainless Steel Pipe
Classification Austenitic Stainless Steel
A814 TP XM-15 Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni
Minimum Value - 1.5 - - - 17 17.5
Maximum Value 0.08 2.5 2 0.03 0.03 19 18.5
A814 TP XM-15 Mechanical Properties
Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
≥515 ≥205
1 Approximate Comparison Table Austenitic Stainless Steel
China Taiwan, China Japan South Korea United States
GB ISC CNS JIS KS ASTM/AISI UNS
06Cr18Ni13Si4
(0Crl8Ni13Si4)
S38148 XM15J1 SUS XM15J1 STS XM15J1 XM15 S38100
2 Approximate Comparison Table Austenitic Heat-Resistant Steel
China Taiwan, China Japan South Korea United States
GB ISC CNS JIS KS ASTM/AISI UNS
06Cr18Ni13Si4
(0Cr18Ni13Si4)
S38148 XM15J1 SUS XM15J1 STS XM15J1 XM15 S38100

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!