Grade grade 7
Corresponding Standard ASME SA-333/SA-333M-2023
Seamless and Welded Steel Pipe for Low-Temperature Service and Other Applications with Required Notch Toughness
Classification Alloy Steel
grade 7 Chemical Element Composition Content (%)
Component C Si Mn P S Ni
Minimum Value - 0.13 - - - 2.03
Maximum Value 0.19 0.32 0.9 0.025 0.025 2.57
grade 7 Mechanical Properties
Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
Impact Energy Absorption
KV2
J
≥450 ≥240 l:≥30;t:≥22 -75°C
≥18
Approximate Comparison Table Processing Titanium and Titanium Alloys
China Japan United States International Organization for Standardization Germany France United Kingdom
GB JIS ASTM ISO DIN EN/DIN W-Nr. NF EN/NF BS EN/BS
TA9 Class 13 Grade 7 Ti-Pd0.2(c) Ti3Pd 3.7255 Ti-Pd0.2(c) Ti-Pd0.2(c)

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!