Grade Grade 3
Corresponding Standard ASTM A334/A334M-2004(R2021)
Seamless and Welded Carbon and Alloy-Steel Tubes for Low-Temperature Service
Classification Alloy Steel
Grade 3 Chemical Element Composition Content (%)
Component C Si Mn P S Ni
Minimum Value - 0.18 0.31 - - 3.18
Maximum Value 0.19 0.37 0.64 0.025 0.025 3.82
Grade 3 Mechanical Properties
Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
Hardness
HBW
Impact Energy Absorption
KV2
J
≥450 ≥240 ≥30 HRB: ≤90
HB: ≤190
-100°C
≥18
Approximate Comparison Table Processing Titanium and Titanium Alloys
China United States International Organization for Standardization Germany
GB ASTM UNS ISO DIN EN/DIN W-Nr.
TA3 Grade 3 R50550 Grade 3(Ti≥99.14) Ti4(Ti≥99.23) 3.7065

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!