Grade 12Ni14
European Standard Steel Grade 1.5637
Corresponding Standard EN 10216-4-2013
Seamless Steel Tubes For Pressure Purpose - Technical Delivery Condition - Part 4: Non-Alloy and Alloy Steel Tubes with Specified Low Temperature Properties
Classification Carbon Steel
12Ni14 Chemical Element Composition Content (%)
Component C Si Mn P S Ni Cu V
Minimum Value - 0.15 0.3 - - 3.25 - -
Maximum Value 0.15 0.35 0.8 0.025 0.005 3.75 0.3 0.05
12Ni14 Mechanical Properties
wall thickness
T
mm
Test Temperature Tensile Strength
σb
Mpa
Specified Plastic Yield Strength
Rp0.2
Mpa
Elongation or Extension Rate
δ
%
Impact Energy Absorption
KV2
J
T≤40 Room Temperature 440~620 ReH or Rp0.2
≥345
l: ≥22
t: ≥20
l: ≥65
t: ≥45
/ T≤25
l: ≥60
t: ≥45
25<T≤40
l: ≥55
t: ≥40
/ T≤25
l: ≥55
t: ≥40
25<T≤40
l: ≥50
t: ≥35
/ T≤25
l: ≥55
t: ≥35
25<T≤40
l: ≥50
t: ≥30
/ T≤25
l: ≥50
t: ≥35
25<T≤45
l: ≥45
t: ≥30
/ T≤25
l: ≥45
t: ≥30
25<T≤45
l: ≥40
t: ≥27
/ T≤25
l: ≥40
t: ≥27
• l=longitudinal;t=transverse
1 Approximate Comparison Table Pressure-Bearing Flat Steel
International Organization for Standardization European Standard
ISO Numerical Grade
12Ni14 1.5637
2 Approximate Comparison Table Pressure-Bearing Flat Steel
China Japan United States International Organization for Standardization European Standard
GB JIS ASTM ISO EN
08Ni3DR
GB/T 713.4-2023
SL3N255
SL3N275
SL3N440
JIS G 3127-2021
3.5%Ni D级
3.5%Ni E级
3.5%Ni F级
ASTM A203/A203M-17
12Ni14
ISO 9328-4-2018
12Ni14
EN 10028-4-2017

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!