Grade X10Ni9
European Standard Steel Grade 1.5682
Corresponding Standard EN 10216-4-2013
Seamless Steel Tubes For Pressure Purpose - Technical Delivery Condition - Part 4: Non-Alloy and Alloy Steel Tubes with Specified Low Temperature Properties
Classification Carbon Steel
X10Ni9 Chemical Element Composition Content (%)
Component C Si Mn P S Ni Cu Mo V
Minimum Value - 0.15 0.3 - - 8.5 - - -
Maximum Value 0.13 0.35 0.8 0.02 0.005 9.5 0.3 0.1 0.05
X10Ni9 Mechanical Properties
wall thickness
T
mm
Test Temperature Tensile Strength
σb
Mpa
Specified Plastic Yield Strength
Rp0.2
Mpa
Elongation or Extension Rate
δ
%
Impact Energy Absorption
KV2
J
T≤40 Room Temperature 690~840 ReH or Rp0.2
≥510
l: ≥20
t: ≥18
l: ≥70
t: ≥50
T≤40 l: ≥70
t: ≥50
T≤40 l: ≥60
t: ≥40
T≤40 l: ≥50
t: ≥35
T≤40 l: ≥40
t: ≥27
• l=longitudinal;t=transverse