Grade HSLAS-F Grade 80
Corresponding Standard ASTM A875/A875-2023
Standard Specification for Steel Sheet, Zinc-5 % Aluminum Alloy-Coated by the Hot-Dip Process
Classification Alloy Steel
HSLAS-F Grade 80 Chemical Element Composition Content (%)
Component C Mn S Cr Ni Cu Mo Ti V Nb
Minimum Value - - - - - - - 0.01 0.01 0.005
Maximum Value 0.15 1.65 0.035 0.15 0.2 0.2 0.16 - - -
① Al、N、B: There is no specified limit, but the analysis shall be reported.
② HSLAS-F steels commonly contain the strengthening elements columbium, vanadium, and titanium added singly or in combination. The minimum requirements only apply to the microalloy elements selected for strengthening of the steel.
③ HSLAS-F steel shall be treated to achieve inclusion control.
HSLAS-F Grade 80 Mechanical Properties
Tensile Strength
σb
ksi
Yield Point
σs
ksi
Elongation or Extension Rate
δ
%
≥90 ≥80 ≥12

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!