Grade 34CrMo4
Other Names
Corresponding Standard ISO 683-1-1987
Heat-Treatable Steels,alloy Steels and Free-Cutting Steels. Part 1:Direct-Hardening Unalloyed and Low-Alloyed Wrought Steel in Form of Different Black Produts
Classification Alloy Steel
34CrMo4 Chemical Element Composition Content (%)
Component C Si Mn P S Cr Mo
Minimum Value 0.3 0.1 0.6 - - 0.9 0.15
Maximum Value 0.37 0.4 0.9 0.035 0.035 1.2 0.3
• The designations are in accordance with the system proposed by ISO/TC 17/SC 2.
• Elements not quoted should not be intentionally added to the steel without the agreement of the purchaser, other than for the purpose of finishing the heat. All reasonable precautions should be taken to prevent the addition, from scrap or other material used in manufacture, of such elements which affect the hardenability, mechanical properties and applicability.
• In the case of the grades with specified hardenability requirements (see tables 5 to 7), except for phosphorous and sulfur, insignificant deviations from the limits for cast analysis are permissible; these deviations shall, however, not exceed in the case of carbon ± 0,01 % (m/m) and in all other cases the values according to table 4.
• For boron-treated steels, see ISO 4954.
• Steels with improved machinability by either lead additions or higher sulfur levels up to about 0,100 % (m/m) S (including controlled sulfide morphology) may be available on request.
34CrMo4 Mechanical Properties
thickness
d
mm
Heat Treatment or Condition
Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
Impact Energy Absorption
KV2
J
d≤16 Qenching + tempering 1000~1200 ≥800 ≥11 KU
≥25
16<d≤4 Qenching + tempering 900~1100 ≥650 ≥12 KU
≥30
40<d≤100 Qenching + tempering 800~950 ≥550 ≥14 KU
≥30
100<d≤160 Qenching + tempering 750~900 ≥500 ≥15 KU
≥30
160<d≤250 Qenching + tempering 700~850 ≥450 ≥15 KU
≥30
1 Approximate Comparison Table Structural Alloy Steel
China Taiwan, China Japan South Korea United States International Organization for Standardization Germany France European Standard Russia Sweden United Kingdom
GB ISC CNS JIS KS ASTM/AISI UNS ISO DIN EN/DIN W-Nr. NF EN/NF EN Numerical Grade GOST SS14 BS EN/BS
35CrMo
35CrMoV
A30352
A31352
SCM435 SCM435
SCM435H
SCM435 4135 G41350 34CrMo4 34CrMo4 1.7220 35CD4 34CrMo4 1.7220 35XM
35ХМФ
2234 708A37
CDS13
2 Approximate Comparison Table Structural Alloy Steel
China Japan United States International Organization for Standardization Germany France European Standard Russia Sweden United Kingdom
GB JIS ASTM ISO DIN EN/DIN NF EN/NF EN Numerical Grade GOST SS BS EN/BS
35CrMo
ZG35CrMo
SCM435H 4135 34CrMo4 34CrMo4 34CD4
35CD4
34CrMo4 1.7220 35KHM
35KHML
2234 708A30
708M32
3 Approximate Comparison Table Cast Steel
China Japan United States International Organization for Standardization Germany France European Standard Russia Sweden United Kingdom
GB JIS ASTM ISO DIN EN/DIN NF EN/NF EN Numerical Grade GOST SS BS EN/BS
ZG35CrMo
35CrMo
SCM435H 4135 34CrMo4 34CrMo4 34CD4
35CD4
34CrMo4 1.7220 35KHM
35KHML
2234 708A30
708M32
4 Approximate Comparison Table Steel for Cold Heading and Cold Extrusion
Japan International Organization for Standardization European Standard
JIS ISO EN Numerical Grade
SCM435
SCM435H
34CrMo4 34CrMo4 1.7220

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!