Grade X2CrNiMoN 17-11-2
European Standard Steel Grade 1.4406
Corresponding Standard EN 10088-3-2005
Stainless Steels--Part 3:Techincal Delivery Conditions for Semi-Finished Products,Bars, Rods, Wire, Sections and Bright Products of Corrosion Resisting Steels for General Purposes
Classification Austenitic Stainless Steel
Properties Corrosion Resistance
X2CrNiMoN 17-11-2 Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni Mo N
Minimum Value - - - - - 16.5 10 2 0.12
Maximum Value 0.03 1 2 0.045 0.03 18.5 12.5 2.5 0.22
① Elements not listed in this table shall not be intentionally added to the steel without the agreement of the purchaser except for finishing the cast. All appropriate precautions are to be taken to avoid the addition of such elements from scrap and other materials used in production which would impair mechanical properties and the suitability of the steel.
Approximate Comparison Table Austenitic Stainless Steel
Japan United States France European Standard United Kingdom
JIS ASTM NF EN/NF EN Numerical Grade BS EN/BS
SUS316LN 316LN Z3CND17-11Az X2CrNiMoN17-11-2 1.4406 316S61

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!