Grade X3CrNiMo13-4
European Standard Steel Grade 1.4313
Corresponding Standard EN 10028-7-2016
Flat Products Made of Steels for Pressure Purposes - Part 7: Stainless Steels
Classification Martensitic Stainless Steel
X3CrNiMo13-4 Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni Mo N
Minimum Value - - - - - 12 3.5 0.3 0.02
Maximum Value 0.05 0.7 1.5 0.04 0.015 14 4.5 0.7 -
X3CrNiMo13-4 Mechanical Properties
condition Heat Treatment or Condition
Tensile Strength
σb
Mpa
Specified Plastic Yield Strength
Rp0.2
Mpa
Elongation or Extension Rate
δ
%
Impact Energy Absorption
KV2
J
P:T ≤ 75 +QT 780~980 ≥650 T ≥3mm
long.+tr.: ≥14①
20°C
long.+ tr.: ≥70
-20°C
long.+ tr.: ≥40
• C=cold rolled strip;H=hot rolled strip;P=hot rolled plate
• +A=Annealed;+AT=Solution annealed
• B=width;T=thick
1 Approximate Comparison Table Other Stainless Steels
Germany France European Standard Sweden United Kingdom
DIN EN/DIN W-Nr. NF EN/NF EN Numerical Grade SS BS EN/BS
X5CrNi 13-4 1.4313 Z25CN 13-4 X3CrNiMo 13-4 1.4313 2385 425C11
2 Approximate Comparison Table Martensitic Stainless Steel
China Japan United States International Organization for Standardization European Standard
GB ISC JIS UNS ISO EN Numerical Grade
04Cr13Ni5Mo S41595 SUS F6NM S41500 X3CrNiMo 13-4 X3CrNiMo 13-4 1.4313
3 Approximate Comparison Table Martensitic Stainless Steel
United States France European Standard Sweden
UNS NF EN/NF EN Numerical Grade SS
S41500 Z6CN13-04 X3CrNiMo13-4 1.4313 2385
4 Approximate Comparison Table Martensitic Stainless Steel
China European Standard
GB EN
0Cr13Ni5Mo X3CrNiMo13-4

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!