Grade X2CrNiMoN18-12-4
European Standard Steel Grade 1.4434
Corresponding Standard EN 10088-2-2024
Stainless Steels - Part 2: Technical Delivery Conditions for Sheet/Plate and Strip of Corrosion Resistant Steels for General Purposes,
Classification Austenitic Stainless Steel
X2CrNiMoN18-12-4 Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni Mo N
Minimum Value - - - - - 16.5 10.5 3 0.1
Maximum Value 0.03 1 2 0.045 0.015 19.5 14 4 0.2
X2CrNiMoN18-12-4 Mechanical Properties
condition Heat Treatment or Condition
Tensile Strength
σb
Mpa
Specified Plastic Yield Strength
Rp0.2
Mpa
Elongation or Extension Rate
δ
%
Impact Energy Absorption
KV2
J
C:T ≤ 8 +AT 570~770 tr©℗.
Rp0.2:≥290
Rp1.0®:≥320
tr.
T<3mm, A80①: ≥35
T≥3mm, A②: ≥35
©
-
H:T ≤ 13.5 +AT 570~770 tr©℗.
Rp0.2:≥270
Rp1.0®:≥310
tr.
T<3mm, A80①: ≥35
T≥3mm, A②: ≥35
©
T>10mm
long.: ≥100
tr.: ≥60
P:T ≤ 75 +AT 540~740 tr©℗.
Rp0.2:≥270
Rp1.0®:≥310
tr.
T<3mm, A80①: ≥40
T≥3mm, A②: ≥40
©
T>10mm
long.: ≥100
tr.: ≥60
Approximate Comparison Table Austenitic Stainless Steel
China Taiwan, China Japan South Korea United States International Organization for Standardization Germany France European Standard
GB ISC CNS JIS KS ASTM UNS ISO DIN EN/DIN W-Nr. NF EN/NF EN Numerical Grade
022Cr19Ni13Mo4N S31753 317LN SUS 317LN STS 317LN 317LN S31753 X2CrNiMoN 18-12-4 X2CrNiMoN 18-12-4 1.4434 X2CrNiMoN 18-12-4 X2CrNiMoN 18-12-4 1.4434

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!