Grade X2CrNiMoN18-12-4
European Standard Steel Grade 1.4434
Corresponding Standard EN 10028-7-2016
Flat Products Made of Steels for Pressure Purposes - Part 7: Stainless Steels
Classification Austenitic Stainless Steel
X2CrNiMoN18-12-4 Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni Mo N
Minimum Value - - - - - 16.5 10.5 3 0.1
Maximum Value 0.03 1 2 0.045 0.015 19.5 14 4 0.2
X2CrNiMoN18-12-4 Mechanical Properties
condition Heat Treatment or Condition
Tensile Strength
σb
Mpa
Specified Plastic Yield Strength
Rp0.2
Mpa
Elongation or Extension Rate
δ
%
Impact Energy Absorption
KV2
J
C:T ≤ 8 +AT 570~770 tr©
Rp0.2:≥290
Rp1.0:≥320
T<3mm, A80①
long.+tr. :≥35;
T≥3mm, A②
long.+tr. :≥35
©
20°C
long.: ≥100
tr.: ≥60
-196°C
tr.: ≥60
H:T ≤ 13.5 +AT 570~770 tr©
Rp0.2:≥270
Rp1.0:≥310
T<3mm, A80①
long.+tr. :≥35;
T≥3mm, A②
long.+tr. :≥35
©
20°C
long.: ≥100
tr.: ≥60
-196°C
tr.: ≥60
P:T ≤ 75 +AT 540~740 tr©
Rp0.2:≥270
Rp1.0:≥310
T<3mm, A80①
long.+tr. :≥40;
T≥3mm, A②
long.+tr. :≥40
©
20°C
long.: ≥100
tr.: ≥60
-196°C
tr.: ≥60
• C=cold rolled strip;H=hot rolled strip;P=hot rolled plate
• +A=Annealed;+AT=Solution annealed
• B=width;T=thick
Approximate Comparison Table Austenitic Stainless Steel
China Taiwan, China Japan South Korea United States International Organization for Standardization Germany France European Standard
GB ISC CNS JIS KS ASTM UNS ISO DIN EN/DIN W-Nr. NF EN/NF EN Numerical Grade
022Cr19Ni13Mo4N S31753 317LN SUS 317LN STS 317LN 317LN S31753 X2CrNiMoN 18-12-4 X2CrNiMoN 18-12-4 1.4434 X2CrNiMoN 18-12-4 X2CrNiMoN 18-12-4 1.4434