Grade X2CrNiMo18-15-4
European Standard Steel Grade 1.4438
Corresponding Standard EN 10028-7-2016
Flat Products Made of Steels for Pressure Purposes - Part 7: Stainless Steels
Classification Austenitic Stainless Steel
X2CrNiMo18-15-4 Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni Mo N
Minimum Value - - - - - 17.5 13 3 -
Maximum Value 0.03 1 2 0.045 0.015 19.5 16 4 0.1
X2CrNiMo18-15-4 Mechanical Properties
condition Heat Treatment or Condition
Tensile Strength
σb
Mpa
Specified Plastic Yield Strength
Rp0.2
Mpa
Elongation or Extension Rate
δ
%
Impact Energy Absorption
KV2
J
C:T ≤ 8 +AT 550~700 tr©
Rp0.2:≥240
Rp1.0:≥270
T<3mm, A80①
long.+tr. :≥35;
T≥3mm, A②
long.+tr. :≥35
©
20°C
long.: ≥100
tr.: ≥60
-196°C
tr.: ≥60
H:T ≤ 13.5 +AT 550~700 tr©
Rp0.2:≥220
Rp1.0:≥260
T<3mm, A80①
long.+tr. :≥35;
T≥3mm, A②
long.+tr. :≥35
©
20°C
long.: ≥100
tr.: ≥60
-196°C
tr.: ≥60
P:T ≤ 75 +AT 520~720 tr©
Rp0.2:≥220
Rp1.0:≥260
T<3mm, A80①
long.+tr. :≥40;
T≥3mm, A②
long.+tr. :≥40
©
20°C
long.: ≥100
tr.: ≥60
-196°C
tr.: ≥60
• C=cold rolled strip;H=hot rolled strip;P=hot rolled plate
• +A=Annealed;+AT=Solution annealed
• B=width;T=thick
Approximate Comparison Table Austenitic Stainless Steel
China Taiwan, China Japan South Korea United States International Organization for Standardization Germany France European Standard Russia Sweden United Kingdom
GB ISC CNS JIS KS ASTM UNS ISO DIN EN/DIN W-Nr. NF EN/NF EN Numerical Grade GOST SS BS EN/BS
022Cr19Ni13Mo3
(00Cr19Ni13Mo3)
S31703 317L SUS 317L STS 317L 317L S31703 X2CrNiMo 19-14-4
X2CrNiMo18-15-4
X2CrNiMo 18-15-4
(X2CrNiMo 18-16)
1.4438 Z2CND 19-15
Z3CND 19-15-04
X2CrNiMo 18-15-4 1.4438 03Х16Н15М3 2367 317S12