Grade SUS 317LN
Other Names
Corresponding Standard JIS G 4304-2021
Hot-Rolled Stainless Steel Plates, Steel and Strip
Classification Austenitic Stainless Steel
Properties Corrosion Resistance
SUS 317LN Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni Mo N
Minimum Value - - - - - 18 11 3 0.1
Maximum Value 0.03 1 2 0.045 0.03 20 15 4 0.22
SUS 317LN Mechanical Properties
Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
Hardness
HBW
≥550 ≥245 ≥40 HBW: ≤217
HRBW: ≤95
HV: ≤220
Approximate Comparison Table Austenitic Stainless Steel
China Taiwan, China Japan South Korea United States International Organization for Standardization Germany France European Standard
GB ISC CNS JIS KS ASTM UNS ISO DIN EN/DIN W-Nr. NF EN/NF EN Numerical Grade
022Cr19Ni13Mo4N S31753 317LN SUS 317LN STS 317LN 317LN S31753 X2CrNiMoN 18-12-4 X2CrNiMoN 18-12-4 1.4434 X2CrNiMoN 18-12-4 X2CrNiMoN 18-12-4 1.4434