Grade 37Cr4
Corresponding Standard ISO 683-1-1987
Heat-Treatable Steels,alloy Steels and Free-Cutting Steels. Part 1:Direct-Hardening Unalloyed and Low-Alloyed Wrought Steel in Form of Different Black Produts
Classification Alloy Steel
37Cr4 Chemical Element Composition Content (%)
Component C Si Mn P S Cr
Minimum Value 0.34 0.1 0.6 - - 0.9
Maximum Value 0.41 0.4 0.9 0.035 0.035 1.2
• The designations are in accordance with the system proposed by ISO/TC 17/SC 2.
• Elements not quoted should not be intentionally added to the steel without the agreement of the purchaser, other than for the purpose of finishing the heat. All reasonable precautions should be taken to prevent the addition, from scrap or other material used in manufacture, of such elements which affect the hardenability, mechanical properties and applicability.
• In the case of the grades with specified hardenability requirements (see tables 5 to 7), except for phosphorous and sulfur, insignificant deviations from the limits for cast analysis are permissible; these deviations shall, however, not exceed in the case of carbon ± 0,01 % (m/m) and in all other cases the values according to table 4.
• For boron-treated steels, see ISO 4954.
• Steels with improved machinability by either lead additions or higher sulfur levels up to about 0,100 % (m/m) S (including controlled sulfide morphology) may be available on request.
37Cr4 Mechanical Properties
thickness
d
mm
Heat Treatment or Condition
Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
Impact Energy Absorption
KV2
J
d≤16 Qenching + tempering 950~1150 ≥750 ≥11 KU
≥20
16<d≤40 Qenching + tempering 850~1000 ≥630 ≥13 KU
≥25
40<d≤100 Qenching + tempering 750~900 ≥510 ≥14 KU
≥25
1 Approximate Comparison Table Alloy Steel for Quenching and Tempering
China International Organization for Standardization European Standard
GB ISO EN Numerical Grade
35Cr 37Cr4 37Cr4 1.7034
2 Approximate Comparison Table Structural Alloy Steel
China Japan United States International Organization for Standardization Germany France European Standard Russia Sweden United Kingdom
GB JIS ASTM ISO DIN EN/DIN W-Nr. NF EN/NF EN Numerical Grade GOST SS BS EN/BS
35Cr SCr435H Gr.5135 37Cr4 37Cr4 1.7034 37Cr4
38C4
37Cr4 1.7034 38KHA
40KH
2245 530A36
530M36
3 Approximate Comparison Table Steel for Cold Heading and Cold Extrusion
International Organization for Standardization European Standard
ISO EN Numerical Grade
37Cr4 37Cr4 1.7034