Grade X1NiCrMoCuN25-20-7
European Standard Steel Grade 1.4539
Corresponding Standard EN 10088-2-2005
Classification Austenitic Stainless Steel
Properties Corrosion Resistance
X1NiCrMoCuN25-20-7 Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni Cu Mo N
Minimum Value - - - - - 19 24 1.2 4 -
Maximum Value 0.02 0.7 2 0.03 0.01 21 26 2 5 0.15
X1NiCrMoCuN25-20-7 Mechanical Properties
thickness
t
mm
Heat Treatment or Condition
Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
Impact Energy Absorption
KV2
J
t≤8; (transverse) Cold Rolled Steel Strip (C) and Solution Annealing 530~730 ②③
≥240
②④⑤
≥35
t≤13.5; (Transverse) Hot Rolled Steel Strip (H) and Solution Annealing 530~730 ≥220 ≥35 ≥60
t≤75; (transverse) Hot Rolled Medium Thick Plate (P) and Solution Annealing 520~720 ≥220 ≥35 ≥60
t≤13.5; (Longitudinal) Hot Rolled Steel Strip (H) and Solution Annealing ≥100
t≤75; (Longitudinal) Hot Rolled Medium Thick Plate (P) and Solution Annealing ≥100
1 Approximate Comparison Table
China Japan United States International Organization for Standardization France European Standard Sweden United Kingdom
GB ISC JIS ASTM/AISI UNS ISO Numerical Grade NF EN/NF EN Numerical Grade SS BS EN/BS
015Cr21Ni26Mo5Cu2 S31782 SUS 890L 904L N08904 X1NiCrMoCu25-20-5 4539-089-04-I Z2NCDU25-20 X1NiCrMoCu25-20-5 1.4539 2562 904S13
2 Approximate Comparison Table
China United States International Organization for Standardization Germany European Standard
GB Commercial Grade UNS ISO Numerical Grade DIN EN/DIN W-Nr. EN Numerical Grade
25-6Mo Incoloy926 N08926 X1NiCrMoCuN25-20-7 4529-089-26-I X1NiCrMoCuN25-20-7 1.4529 X1NiCrMoCuN25-20-7 1.4529
3 Approximate Comparison Table
United States European Standard
ASTM EN Numerical Grade
N08926
NO8367
X1NiCrMoCuN25-20-7 1.4529

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!