Grade 12Cr1MoVG
China ISC A31128
Corresponding Standard GB 5310-1995
Seamless Steel Tubes and Pipes for High Pressure Boiler
Classification Alloy Steel
12Cr1MoVG Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni Cu Mo V
Minimum Value 0.08 0.17 0.4 - - 0.9 - - 0.25 0.15
Maximum Value 0.15 0.37 0.7 0.03 0.03 1.2 0.3 0.2 0.35 0.3
• Steel produced by oxygen converter and secondary refining outside the furnace has a nitrogen content not exceeding 0.008%
12Cr1MoVG Mechanical Properties
Heat Treatment or Condition
Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
Impact Energy Absorption
KV2
J
Longitudinal Normalizing + Tempering
Quenching + Tempering
470~640 ≥255 ≥21 ≥35
Transverse Normalizing + Tempering
Quenching + Tempering
≥440 ≥255 ≥19 ≥27
12Cr1MoVG Corresponding Standards(Same grade name, different standards)