Grade 12Cr2MoWVTiB
China ISC A32128
Corresponding Standard GB 5310-1995
Seamless Steel Tubes and Pipes for High Pressure Boiler
Classification Alloy Steel
12Cr2MoWVTiB Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni Cu Mo Ti W V B
Minimum Value 0.08 0.45 0.45 - - 1.6 - - 0.5 0.08 0.3 0.28 0.002
Maximum Value 0.15 0.75 0.65 0.03 0.03 2.1 0.3 0.2 0.65 0.18 0.55 0.42 0.008
• Steel produced by oxygen converter and secondary refining outside the furnace has a nitrogen content not exceeding 0.008%
12Cr2MoWVTiB Mechanical Properties
Heat Treatment or Condition
Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
Impact Energy Absorption
KV2
J
Normalizing + Tempering:
Normalizing temperature 1020~1060°C,
Tempering temperature 760~790°C
540~735 ≥345 long. ≥18 long. ≥35
tr. ≥27
12Cr2MoWVTiB Corresponding Standards(Same grade name, different standards)