Grade Grade F20
USA UNS N08020
Other Names
Corresponding Standard ASTM A965/A965M-2025
Standard Specification for Steel Forgings, Austenitic, for Pressure and High Temperature Parts
Classification Austenitic Stainless Steel
Grade F20 Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni Cu Mo More
Minimum Value - - - - - 19 32 3 2 Nb:8×C~1.00
Maximum Value 0.07 1 2 0.045 0.035 21 38 4 3
Grade F20 Mechanical Properties
Tensile Strength
σb
Mpa
Specified Plastic Yield Strength
Rp0.2
Mpa
Elongation or Extension Rate
δ
%
Reduction of Area
ψ
%
≥550 ≥240 ≥30 ≥50
1 Approximate Comparison Table Corrosion-Resistant Alloy
China United States Germany
GB ISC Commercial Grade UNS DIN EN/DIN W-Nr.
NS 1403
(NS143)
(0Cr20Ni35Mo3Cu4Nb)
H 08020
H 01403
Alloy 20cb3
Carpenter 20Cb3
N 08020 NiCr20CuMo 2.4660
2 Approximate Comparison Table Austenitic Stainless Steel
United States International Organization for Standardization European Standard
UNS ISO Numerical Grade Numerical Grade
N08020 X4NiCrCuMo35-20-4-3 4657-080-20-U (1.4657)

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!