Grade Grade FNIC11
USA UNS N08811
Other Names
Corresponding Standard ASTM A965/A965M-2025
Standard Specification for Steel Forgings, Austenitic, for Pressure and High Temperature Parts
Classification Austenitic Stainless Steel
Grade FNIC11 Chemical Element Composition Content (%)
Component Fe C Si Mn P S Cr Ni Cu Ti Al
Minimum Value 39.5 0.06 - - - - 19 30 - 0.25 0.25
Maximum Value - 0.1 1 1.5 0.04 0.015 23 35 0.75 0.6 0.6
① Ti+Al: 0.85%~1.20%.
Grade FNIC11 Mechanical Properties
Tensile Strength
σb
Mpa
Specified Plastic Yield Strength
Rp0.2
Mpa
Elongation or Extension Rate
δ
%
≥450 ≥170 ≥30
1 Approximate Comparison Table Corrosion-Resistant Alloy
China United States
GB ISC Commercial Grade UNS
NS 1104 H 08811 Incoloy 800HT N 08811
2 Approximate Comparison Table Austenitic Stainless Steel
United States International Organization for Standardization European Standard
UNS ISO Numerical Grade Numerical Grade
N08811 X8NiCrAlTi33-21 4959-088-11-U 1.4959
3 Approximate Comparison Table Corrosion-Resistant Alloy
United States Germany
Commercial Grade UNS DIN EN/DIN W-Nr.
Incoloy 800HT N08811 X8NiCrAlTi32-21 1.4959

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!