Grade K213
Old Grade
Corresponding Standard GJB 5512.1-2005
Specification for Superalloy and High Temperature Intermetallic Materials Master Alloys for Castings —— Part 1: Superalloy Master Alloys for Conventional Investment Castings
Classification Special Alloy Steel
Properties Corrosion Resistance
K213 Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni Ti W B Al More
Minimum Value - - - - - 14 34 3 4 0.05 1.5 Fe:Remainder
Maximum Value 0.1 0.5 0.5 0.015 0.015 16 38 4 7 0.1 2
K213 Mechanical Properties
Test Temperature Heat Treatment or Condition
Tensile Strength
σb
Mpa
Elongation or Extension Rate
δ
%
Reduction of Area
ψ
%
试样 Hold at 1100±10°C for 4 h and then air cool ≥628 ≥6 ≥10
试样 Hold at 1100±10°C for 5 h and then air cool ≥528 ≥4 ≥8
K213 Corresponding Standards(Same grade name, different standards)