Grade P235TR2
European Standard Steel Grade 1.0255
Corresponding Standard EN 10216-1-2013
Seamless steel tubes for pressure purposes - Technical delivery conditions - Part 1: Non-alloy steel tubes with specified room temperature properties
Classification Carbon Steel
P235TR2 Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni Cu Mo Ti V Nb Al * More
Minimum Value - - - - - - - - - - - - 0.02 Cr+Cu+Mo+Ni ≤0.7%
Maximum Value 0.16 0.35 1.2 0.025 0.015 0.3 0.3 0.3 0.08 0.04 0.02 0.01 -
* This requirement is not applicable provided the steel contains a sufficient amount of other nitrogen binding elements which shall be reported.
P235TR2 Mechanical Properties
wall thickness
T
mm
Tensile Strength
σb
Mpa
Specified Plastic Yield Strength
Rp0.2
Mpa
Elongation or Extension Rate
δ
%
Impact Energy Absorption
KV2
J
T≤16 360~500 ReH
≥235
l:≥25;t:≥23 0°C:
l:≥40;t:≥27
-10°C:
l:≥28
16<T≤40 360~500 ReH
≥225
l:≥25;t:≥23 0°C:
l:≥40;t:≥27
-10°C:
l:≥28
40<T≤60 360~500 ReH
≥215
l:≥25;t:≥23 0°C:
l:≥40;t:≥27
-10°C:
l:≥28
• l=longitudinal;t=transverse
P235TR2 Corresponding Standards(Same grade name, different standards)

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!