Grade 13CrMo4-5
European Standard Steel Grade 1.7335
Corresponding Standard EN 10216-2-2024
Seamless Steel Tubes for Pressure Purposes - Technical Delivery Conditions - Part 2: Non-Alloy and Alloy Steel Tubes with Specified Elevated Temperature Properties
Classification Alloy Steel
13CrMo4-5 Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni Cu Mo Al
Minimum Value 0.1 - 0.4 - - 0.7 - - 0.4 -
Maximum Value 0.17 0.35 0.7 0.025 0.01 1.15 0.3 0.3 0.6 0.04
13CrMo4-5 Mechanical Properties
wall thickness
T
mm
Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
Impact Energy Absorption
KV2
J
T≤16 440~590 ReH
≥290
l: ≥22;t: ≥20 20°C:
l: ≥40;t: ≥27
16<T≤40 440~590 ReH
≥290
l: ≥22;t: ≥20 20°C:
l: ≥40;t: ≥27
40<T≤60 440~590 ReH
≥280
l: ≥22;t: ≥20 20°C:
l: ≥40;t: ≥27
• l = longitudinal; t = transverse.
1 Approximate Comparison Table Steel Plate for Boilers and Pressure Vessels
China United States International Organization for Standardization European Standard Russia
GB ASTM ISO EN Numerical Grade GOST
15CrMoR
GB/T 713.2-2023
SA387 Gr.12
ASME Ⅱ-A-2021
13CrMo4-5
ISO 9328-2018
13CrMo4-5
EN 10028-2017
1.7335 12ХМ
2 Approximate Comparison Table Structural Alloy Steel
China Japan United States International Organization for Standardization Germany France European Standard Russia Sweden United Kingdom
GB JIS ASTM ISO DIN EN/DIN NF EN/NF EN Numerical Grade GOST SS BS EN/BS
12CrMo SFVAF12 A387Gr.12
Gr.P12
F32
P32
13CrMo4-4 15CD2.05
15CD4-05
15CD4-5
13CrMo4-5 1.7335 12KHM
15KHM
2216 620
620-440
620Gr.27
3 Approximate Comparison Table Seamless Steel Tubes and Pipes for High Pressure Boiler
China United States European Standard
GB ISC ASTM/AISI EN
15CrMoG A30158 SA-213 T12
SA-213 T12
13CrMo4-5

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!