Grade STBA12
Corresponding Standard JIS G 3462-2019
Alloy Steel Tubes for Boiler and Heat Exchanger
Classification Alloy Steel
STBA12 Chemical Element Composition Content (%)
Component C Si Mn P S Mo
Minimum Value 0.1 0.1 0.3 - - 0.45
Maximum Value 0.2 0.5 0.8 0.035 0.035 0.65
• Addition of Cr is permitted to a level where chemical composition of the grade concerned remains distinguishable, after the addition of Cr, from those of all other grades.
STBA12 Mechanical Properties
outside diameter
d
mm
Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
d<10 ≥380 ≥205 ≥22
10≤d<20 ≥380 ≥205 ≥25
d≥20 ≥380 ≥205 ≥30
Approximate Comparison Table Structural Alloy Steel
Japan United States International Organization for Standardization Germany France European Standard Sweden United Kingdom
JIS ASTM ISO DIN EN/DIN NF EN/NF EN Numerical Grade SS BS EN/BS
STBA12 A204Gr.A
A204Gr.B
F26
P26
TS26
15Mo3
16Mo3
15D3 16Mo3 1.5415 2912 1503-243B
240
243

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!