Grade CP1
USA UNS J12521
Corresponding Standard ASTM A426/A426M-2025
Standard Specification for Centrifugally Cast Ferritic Alloy Steel Pipe for High-Temperature Service
Classification Cast Steel
CP1 Chemical Element Composition Content (%)
Component C Si Mn P S Mo
Minimum Value - 0.1 0.3 - - 0.44
Maximum Value 0.25 0.5 0.8 0.03 0.025 0.65
CP1 Mechanical Properties
Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
Reduction of Area
ψ
%
Hardness
HBW
≥450 ≥240 ≥24 ≥35 ≤201