USA UNS N06058
Corresponding Standard ASTM B 574-2023
Standard Specification for Low-Carbon Nickel-Chromium-Molybdenum, Low-Carbon Nickel-Molybdenum-Chromium, Low-Carbon Nickel-Molybdenum-Chromium-Tantalum, Low-Carbon Nickel-Chromium-Molybdenum-Copper, and Low-Carbon Nickel-Chromium-Molybdenum-Tungsten Alloy
Classification Nickel and Nickel Alloys
Density 8.8 g/cm3
Chemical Element Composition Content (%)
Component Fe C Si Mn P S Cr Cu Mo N W Co Al More
Minimum Value - - - - - - 20 - 18.5 0.02 - - - Ni: remainder
Maximum Value 1.5 0.01 0.1 0.5 0.015 0.01 23 0.5 21 0.15 0.3 0.3 0.4
Mechanical Properties
Heat Treatment or Condition
Tensile Strength
σb
Mpa
Specified Plastic Yield Strength
Rp0.2
Mpa
Elongation or Extension Rate
δ
%
Hot or Cold Finished, Solution Annealed ≥760 ≥360 ≥40

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!