USA UNS N06045
Corresponding Standard ASTM B 166-2025
Standard Specification for Nickel-Chromium-Aluminum Alloy, Nickel-Chromium-Iron Alloys, Nickel-Chromium-Cobalt-Molybdenum Alloy, Nickel-Iron-Chromium-Tungsten Alloy, and Nickel-Chromium Molybdenum-Copper Alloy Rod, Bar, and Wire
Classification Nickel and Nickel Alloys
Properties Corrosion Resistance
Chemical Element Composition Content (%)
Component Fe C Si Mn P S Cr Ni Cu Ce
Minimum Value 21 0.05 2.5 - - - 26 45 - 0.03
Maximum Value 25 0.12 3 1 0.02 0.01 29 - 0.3 0.09
Mechanical Properties
Heat Treatment or Condition
Tensile Strength
σb
Mpa
Specified Plastic Yield Strength
Rp0.2
Mpa
Elongation or Extension Rate
δ
%
All products. all sizes Cold-worked (annealed) or hot-worked (annealed) ≥620 ≥240 ≥35
Rods and bars. all sizes hot-worked (annealed), High-temperature annealed condition ≥517 ≥207 ≥30

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!