USA UNS S34800
ASTM
Specification or Grade
348
Corresponding Standard ASTM A 473-2024(a)
Stainless Steel Forgings
Classification Austenitic Stainless Steel
Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni Co Ta More
Minimum Value - - - - - 17 9 - - Cb+Ta:10C min
Maximum Value 0.08 1 2 0.045 0.03 19 13 0.2 0.1
Mechanical Properties
Heat Treatment or Condition
Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
Reduction of Area
ψ
%
A - annealed ≥515 ≥205 ≥40 ≥50

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!