USA UNS S41500
Corresponding Standard ASTM A 473-2024(a)
Stainless Steel Forgings
Classification Martensitic Stainless Steel
Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni Mo
Minimum Value - - 0.5 - - 11.5 3.5 0.4
Maximum Value 0.05 0.6 1 0.03 0.03 14 5.5 0.8
Mechanical Properties
Heat Treatment or Condition
Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
Reduction of Area
ψ
%
Hardness
HBW
Normalizing + Tempering ≥795 ≥620 ≥15 ≥45 ≤295
1 Approximate Comparison Table Martensitic Stainless Steel
China Japan United States International Organization for Standardization European Standard
GB ISC JIS UNS ISO EN Numerical Grade
04Cr13Ni5Mo S41595 SUS F6NM S41500 X3CrNiMo 13-4 X3CrNiMo 13-4 1.4313
2 Approximate Comparison Table Martensitic Stainless Steel
United States France European Standard Sweden
UNS NF EN/NF EN Numerical Grade SS
S41500 Z6CN13-04 X3CrNiMo13-4 1.4313 2385

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!