Grade A308 SS Grade 170
Corresponding Standard ASTM A308/A308M-2010
Standard Specification for Steel Sheet, Terne (Lead-Tin Alloy) Coated by the Hot-Dip Process
Classification Carbon Steel
A308 SS Grade 170 Chemical Element Composition Content (%)
Component C Mn P S Cr Ni Cu Mo Ti V Cb
Minimum Value - - - - - - - - - - -
Maximum Value 0.2 0.6 0.04 0.04 0.15 0.2 0.2 0.06 0.025 0.008 0.008
① For steels containing more than 0.02 % carbon, titanium is permitted to 0.025 % provided the ratio of % titanium to % nitrogen does not exceed 3.4.
A308 SS Grade 170 Mechanical Properties
Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
≥290 ≥170 ≥26