USA UNS S38400
AISI
American Iron and Steel Institute
384
Corresponding Standard ASTM A 493-2025
Standard Specification for Stainless Steel Wire and Wire Rods for Cold Heading and Cold Forging
Classification Austenitic Stainless Steel
Properties Corrosion Resistance Good Forgability
Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni
Minimum Value - - - - - 15 17
Maximum Value 0.04 1 2 0.045 0.03 17 19
Mechanical Properties
diameter
d
mm
Heat Treatment or Condition
Tensile Strength
σb
Mpa
Wires, rebar; d≥2.5 Annealing ≤550
Wires, rebar; d≥2.5 Light Drawing ≤585
Approximate Comparison Table Austenitic Stainless Steel
China Japan United States International Organization for Standardization European Standard
GB ISC JIS UNS ISO Numerical Grade Numerical Grade
06Ni18Cr16 S38408 SUS384 S38400 X3NiCr18-16 4389-384-00-I (1.4389)

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!