Grade EN-GJLA-XNiCuCr15-6-2
European Standard Steel Grade 5.1500
Corresponding Standard EN 13835-2012
Founding - Austenitic Cast Irons
Classification cast Iron
EN-GJLA-XNiCuCr15-6-2 Chemical Element Composition Content (%)
Component C Si Mn P Cr Ni Cu
Minimum Value - 1 0.5 - 1 13.5 5.5
Maximum Value 3 2.8 1.5 0.25 3.5 17.5 7.5
EN-GJLA-XNiCuCr15-6-2 Mechanical Properties
Tensile Strength
σb
Mpa
≥170
New and Old Grade Replacement List
Approximate Comparison Table Cast Iron
United States International Organization for Standardization Germany France European Standard United Kingdom
ASTM ISO DIN EN/DIN NF EN/NF EN Numerical Grade BS EN/BS
Type1 L-NiCuCr15-6-2
Ni-Resist1
GGL-NiCuCr15-6-2 FGL-Ni15Cu6Cr2 EN-GJLA-XNiCuCr15-6-2 EN-JL3011 AUS101A
F1
L-NiCuCr15-6-2

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!