Grade X6CrNiTi 18 10
Germany W-Nr. 1.4541
Corresponding Standard DIN 1654-5-1989
Cold heading and Cold Extruding Steels Technical Delivery Conditions for Stainless Steels
Classification Austenitic Stainless Steel
X6CrNiTi 18 10 Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni More
Minimum Value - - - - - 17 9 Ti:5C~0.8
Maximum Value 0.08 1 2 0.045 0.03 19 12
X6CrNiTi 18 10 Mechanical Properties
condition Heat Treatment or Condition
Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
Reduction of Area
ψ
%
Impact Energy Absorption
KV2
J
Steel quenching or quenching + peeling ≤680 ≥55
Steel Cold draw + quenching ≤680 ≥55
Steel Cold draw + quenching + slightly cold redraw (K+GKZ+K) ≤730 ≥55
Steel quenching 500~730 ≥200 ≥40 ≥60
New and Old Grade Replacement List
1 Approximate Comparison Table Austenitic Stainless Steel
China Taiwan, China Japan South Korea United States International Organization for Standardization Germany France European Standard Russia Sweden United Kingdom
GB ISC CNS JIS KS ASTM UNS ISO Numerical Grade DIN EN/DIN W-Nr. NF EN/NF EN Numerical Grade GOST SS BS EN/BS
06Cr18Ni11Ti S32168 321 SUS 321 STS 321 321 S32100 X6CrNiTi 18-10 4541-321-00-I X6CrNiTi 18-10
(X10CrNiTi 18-9)
1.4541 Z6CNT 18-10 X6CrNiTi 18-10 1.4541 09Х18Н10Т
Х18Н10Т
2337 321S12
321S31
2 Approximate Comparison Table Austenitic Heat-Resistant Steel
China Taiwan, China Japan South Korea United States International Organization for Standardization Germany France European Standard Russia Sweden United Kingdom
GB ISC CNS JIS KS ASTM UNS ISO DIN EN/DIN W-Nr. NF EN/NF EN Numerical Grade GOST SS BS EN/BS
06Cr18Ni11Ti
(0Cr18Ni11Ti)
S32168 321 SUS 321 STS 321 321 S32100 X6CrNiTi 18-10 X6CrNiTi 18-10
(X10CrNiTi 18-9)
1.4541 Z6CNT 18-10 X6CrNiTi 18-10 1.4541 09Х18Н10Т 2337 321S12
321S31
X6CrNiTi1810 Corresponding Standards(Same grade name, different standards)

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!