Grade X2CrNiMo 17-12-2
Germany W-Nr. 1.4404
Corresponding Standard DIN EN 10263-5-2002
Steel Rod, Bars and Wire for Cold Heading and Cold Extrusion - Part 5: Technical Delivery Conditions for Stainless Steels
Classification Austenitic Stainless Steel
Properties Corrosion Resistance
X2CrNiMo 17-12-2 Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni Cu Mo N
Minimum Value - - - - - 16.5 10 - 2 -
Maximum Value 0.03 1 2 0.045 0.03 18.5 13 1 2.5 0.11
1 Approximate Comparison Table Other Stainless Steels
Germany France European Standard United Kingdom
DIN EN/DIN W-Nr. NF EN/NF EN Numerical Grade BS EN/BS
X2CrNiMo 17-13-2
(X2CrNiMo 18-10)
1.4404 Z2CND 17-12 X2CrNiMo 17-12-2 1.4404 316S11
2 Approximate Comparison Table Heat-Resistant Cast Steels and Alloys
United States Germany France
ASTM UNS DIN EN/DIN W-Nr. NF EN/NF
CF-3
CF-3M
J92700
J92800
G-X2CrNiMo18 10 1.4404 Z2CND18.12-M
Z3CND19.10-M
X2CrNiMo17-12-2 Corresponding Standards(Same grade name, different standards)

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!