Grade X2CrNiMo 17-12-3
Germany W-Nr. 1.4432
Corresponding Standard DIN EN 10263-5-2002
Steel Rod, Bars and Wire for Cold Heading and Cold Extrusion - Part 5: Technical Delivery Conditions for Stainless Steels
Classification Austenitic Stainless Steel
Properties Corrosion Resistance
X2CrNiMo 17-12-3 Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni Cu Mo N
Minimum Value - - - - - 16.5 10.5 - 2.5 -
Maximum Value 0.03 1 2 0.045 0.015 18.5 13 1 3 0.11