Grade X3CrNiCu18-9-4
Germany W-Nr. 1.4567
Corresponding Standard DIN EN 10263-5-2002
Steel Rod, Bars and Wire for Cold Heading and Cold Extrusion - Part 5: Technical Delivery Conditions for Stainless Steels
Classification Austenitic Stainless Steel
Properties Corrosion Resistance
X3CrNiCu18-9-4 Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni Cu N
Minimum Value - - - - - 17 8.5 3 -
Maximum Value 0.04 1 2 0.045 0.03 19 10.5 4 0.11
New and Old Grade Replacement List
Approximate Comparison Table Austenitic Stainless Steel
China Taiwan, China Japan South Korea United States International Organization for Standardization Germany France European Standard
GB ISC CNS JIS KS ASTM/AISI UNS ISO Numerical Grade DIN EN/DIN W-Nr. NF EN/NF EN Numerical Grade
06Cr18Ni9Cu3 S30488 XM7 SUS XM7 STS XM7 XM7 S30430 X3CrNiCu 18-9-4 4567-304-30-I X3CrNiCu 18-9 1.4567 Z3CNU 18-10 X3CrNiCu 18-9-4 1.4567

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!