Grade GX40CrSi17
Germany W-Nr. 1.4740
Corresponding Standard DIN EN 10295-2003
Heat Resistant Steel Castings
Classification Cast Steel
Density 7.7 g/cm3
GX40CrSi17 Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni Cu * Mo W * V * Nb * Co *
Minimum Value 0.3 1 - - - 16 - - - - - - -
Maximum Value 0.5 2.5 1 0.04 0.03 19 1 0.2 0.5 0.2 0.08 0.2 0.5
GX40CrSi17 Mechanical Properties
condition Test Temperature Heat Treatment or Condition
Specified Plastic Yield Strength
Rp0.2
Mpa
Hardness
HBW
铸钢 Room Temperature Annealing (+A) ≤300
铸钢 Creep Strength for 1%-10000h
22
铸钢 Creep Strength for 1%-10000h
9
铸钢 Creep Strength for 1%-10000h
3.5
铸钢 Creep Strength for 1%-10000h
1
Approximate Comparison Table Heat-Resistant Cast Steels and Alloys
China Taiwan, China Japan South Korea International Organization for Standardization Germany France United Kingdom
GB ISC CNS JIS KS ISO DIN EN/DIN W-Nr. NF EN/NF BS EN/BS
ZG40Cr17Si2 C54830 ≈SCH 1 SCH 5 ≈HRSC 1 GX40CrSi17 GX40CrSi17 1.4740 GX40CrSi17 GX40CrSi17
GX40CrSi17 Corresponding Standards(Same grade name, different standards)

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!