Grade C16E4
ISO Numeric Designation 3
Corresponding Standard ISO 683-11-1987
heat-treatable steels, alloy steels and free-cutting steels -- part 11: case-hardening steels
Classification Alloy Steel
Properties Carburizing Ability
C16E4 Chemical Element Composition Content (%)
Component C Si Mn P S
Minimum Value 0.12 0.15 0.6 - -
Maximum Value 0.18 0.4 0.9 0.035 0.035
1 Approximate Comparison Table
China Taiwan, China Japan South Korea United States International Organization for Standardization Germany France European Standard Russia Sweden United Kingdom
GB ISC CNS JIS KS ASTM UNS ISO DIN EN/DIN W-Nr. NF EN/NF EN Numerical Grade GOST SS BS EN/BS
12Cr13
(1Cr13)
S41010 410 SUS 410 STS 410 410 S41000 X12Cr 13
3
(ISO 683-13-1986)
X10Cr 13 1.4006 Z12C 13 X12Cr 13 1.4006 12Х13 2302 410S21
2 Approximate Comparison Table
International Organization for Standardization France European Standard United Kingdom
ISO NF EN/NF EN Numerical Grade BS EN/BS
C16E4 XC18 C16E 1.1148 080M15
3 Approximate Comparison Table
China United States International Organization for Standardization France
GB ASTM/AISI ISO NF EN/NF
0Cr15Ni7Mo2Al 632 3
(ISO 683-13-1986)
Z8CND15.7