Grade 800H
USA UNS N08810
Corresponding Standard ASTM A213/A213M-2025
Seamless Ferritic and Austenitic Alloy-Steel Boiler, Superheater, and Heat-Exchanger Tubes
Classification Austenitic Stainless Steel
800H Chemical Element Composition Content (%)
Component Fe C Si Mn P S Cr Ni Cu Ti Al
Minimum Value 39.5 0.05 - - - - 19 30 - 0.15 0.15
Maximum Value - 0.1 1 1.5 0.045 0.015 23 35 0.75 0.6 0.6
① Iron shall be determined arithmetically by difference of 100 minus the sum of the other specified elements.
800H Mechanical Properties
Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
Hardness
HBW
≥450 ≥170 ≥30 ≤192
1 Approximate Comparison Table Corrosion-Resistant Alloy
China United States Germany United Kingdom
GB ISC Commercial Grade UNS DIN EN/DIN W-Nr. BS EN/BS
NS 1102
(NS 112)
(1Cr20Ni32AlTi)
H 08810
H 01102
Incoloy 800H N 08810 X10NiCrAlTi 32-20 1.4876 NA 15
2 Approximate Comparison Table Austenitic Stainless Steel
Japan United States International Organization for Standardization European Standard
JIS UNS ISO Numerical Grade Numerical Grade
NCF800H N08810 X7NiCrAlTi33-21 4959-088-10-U 1.4959
3 Approximate Comparison Table Corrosion-Resistant Alloy
China United States Germany United Kingdom
GB Commercial Grade UNS DIN EN/DIN W-Nr. BS EN/BS
NS112 Incoloy 800H N08810 X5NiCrAlTi31-20 1.4958 NA15(H)