Grade X6CrNiNb18-10
Old Grade
Corresponding Standard ISO 9327(-5)-1999
Steel forgings and rolled or forged bars for pressure purposes-Technical delivery conditions-Part 5:Stainless steels
Classification Other metal materials
Properties Corrosion Resistance
X6CrNiNb18-10 Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni More
Minimum Value - - - - - 17 9 Nb:10×C ~ 1.00
Maximum Value 0.08 1 2 0.045 0.03 19 12
X6CrNiNb18-10 Mechanical Properties
thickness
t
mm
Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
t≤450 510~710 ≥205 ≥30
1 Approximate Comparison Table Austenitic Stainless Steel
China Taiwan, China Japan South Korea United States International Organization for Standardization Germany France European Standard Russia Sweden United Kingdom
GB ISC CNS JIS KS ASTM/AISI UNS ISO DIN EN/DIN W-Nr. NF EN/NF EN Numerical Grade GOST SS BS EN/BS
06Cr18Ni11Nb S34778 347 SUS 347 STS 347 347 S34700 X6CrNiNb 18-10 X6CrNiNb 18-10
(X10CrNiNb18-9)
1.4550 Z6CNNb 18-10 X6CrNiNb 18-10 1.4550 08Х18Н12Б 2338 347S17
347S31
2 Approximate Comparison Table Austenitic Heat-Resistant Steel
China Taiwan, China Japan South Korea United States International Organization for Standardization Germany France European Standard Russia Sweden United Kingdom
GB ISC CNS JIS KS ASTM/AISI UNS ISO DIN EN/DIN W-Nr. NF EN/NF EN Numerical Grade GOST SS BS EN/BS
06Cr18Ni11Nb
(0Cr18Ni11Nb)
S34778 347 SUS 347 STS 347 347 S34700 X6CrNiNb 18-10 X6CrNiNb 18-10
(X10CrNiNb18-9)
1.4550 Z6CNNb 18-10 X6CrNiNb 18-10 1.4550 08Х18Н12Б 2338 347S17
347S31
3 Approximate Comparison Table Austenitic Stainless Steel
China International Organization for Standardization European Standard
GB ISO EN
0Cr18Ni10Nb X6CrNiNb18-10 X6CrNiNb18-10

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!