Grade X2CrNiMoN17-13
Corresponding Standard ISO 9327(-5)-1999
Steel forgings and rolled or forged bars for pressure purposes-Technical delivery conditions-Part 5:Stainless steels
Classification Other metal materials
Properties Corrosion Resistance
X2CrNiMoN17-13 Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni Mo N
Minimum Value - - - - - 16.5 11.5 2.5 0.12
Maximum Value 0.03 1 2 0.045 0.03 18.5 14.5 3 0.22
X2CrNiMoN17-13 Mechanical Properties
thickness
t
mm
Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
t≤160 580~780 ≥280 ≥30

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!