Grade X2CrNiN23-4
Corresponding Standard ISO 9327(-5)-1999
Steel forgings and rolled or forged bars for pressure purposes-Technical delivery conditions-Part 5:Stainless steels
Classification Other metal materials
Properties Corrosion Resistance
X2CrNiN23-4 Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni Cu Mo N
Minimum Value - - - - - 22 3.5 - - 0.05
Maximum Value 0.03 1 2.5 0.035 0.02 24 5 0.6 0.6 0.2
X2CrNiN23-4 Mechanical Properties
thickness
t
mm
Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
t≤160 600~820 ≥400 ≥25
1 Approximate Comparison Table Austenitic-Ferritic Stainless Steel
China United States International Organization for Standardization European Standard
GB ISC ASTM UNS ISO EN Numerical Grade
022Cr23Ni4MoCuN S23043 2304 S32304 X2CrNiN 23-4 X2CrNiN 23-4 1.4362
2 Approximate Comparison Table Austenitic-Ferritic Stainless Steel
China United States International Organization for Standardization United Kingdom
GB ISC AISI UNS ISO Numerical Grade BS EN/BS
022Cr23Ni4MoCuN
(GB/T 39033)
S23043 2304 S32304
(ASTM A595-16)
X2CrNiN23-4
(ISO 15510:2014)
4362-323-04-Ⅰ X2CrNiN23-4/1.4362
(BS EN 10083:2014)