Grade X7CrNiMoBNb 16-16
European Standard Steel Grade 1.4986
Corresponding Standard EN 10269-2013
Steels and Nickel Alloys for Fasteners with Specified Elevated and/or Low Temperature Properties
Classification Austenitic Stainless Steel
Properties Corrosion Resistance
Density 7.9 g/cm3
X7CrNiMoBNb 16-16 Chemical Element Composition Content (%)
Component C Si Mn P S * Cr Ni Mo B More
Minimum Value 0.04 0.3 - - - 15.5 15.5 1.6 0.05 Nb+Ta: 10×C~1.20
Maximum Value 0.1 0.6 1.5 0.045 0.015 17.5 17.5 2 0.1
X7CrNiMoBNb 16-16 Mechanical Properties
diameter
d
mm
Heat Treatment or Condition
Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
Impact Energy Absorption
KV2
J
d≤100 +WW+P 650~850 ≥500 ≥16 ≥50