USA UNS G10700
AISI
American Iron and Steel Institute
1070
Corresponding Standard ASTM A29/A29M-2023
General Requirements for Steel Bars, Carbon and Alloy, Hot-Wrought
Classification Carbon Steel
Chemical Element Composition Content (%)
Component C Mn P S
Minimum Value 0.65 0.6 - -
Maximum Value 0.75 0.9 0.04 0.05
① When silicon is required, the following ranges and limits are commonly specified: 0.10 %, max. 0.10 % to 0.20 %, 0.15 % to 0.35 %, 0.20 % to 0.40 %, or 0.30 % to 0.60%.
② Copper can be specified when required as 0.20 % minimum.
③ When lead is required as an added element to a standard steel, a range of 0.15 % to 0.35 % inclusive is specified. Such a steel is identified by inserting the letter L between the second and third numerals of the grade designation, for example, 10L45. A cast or heat analysis is not determinable when lead is added to the ladle stream.
④ When boron treatment for killed steels is specified, the steels can be expected to contain 0.0005 % to 0.003 % boron. If the usual titanium additive is not permitted, the steels can be expected to contain up to 0.005 % boron.
⑤ The elements bismuth, calcium, selenium, or tellurium may be added as agreed upon between purchaser and supplier.
1 Approximate Comparison Table Spring Steel
China United States International Organization for Standardization France Russia Sweden United Kingdom
GB ISC AISI UNS ISO NF EN/NF GOST SS14 BS EN/BS
70 U20702 1070 G10700 Type DC XC70 70 1778 070A72
2 Approximate Comparison Table Wrought Aluminum and Aluminum Alloy
China Japan United States International Organization for Standardization Germany European Standard Russia
GB JIS ASTM UNS ISO Numerical Grade DIN EN/DIN W-Nr. EN GOST
1070 1070
A91070
1070 A91070 Al99.7 A91070 Al99.7 3.0275
A91070
EN-AW-Al99.7 АД00Е