USA UNS G10800
AISI
American Iron and Steel Institute
1080
Corresponding Standard ASTM A29/A29M-2023
General Requirements for Steel Bars, Carbon and Alloy, Hot-Wrought
Classification Carbon Steel
Properties Good Forgability
Chemical Element Composition Content (%)
Component C Mn P S
Minimum Value 0.75 0.6 - -
Maximum Value 0.88 0.9 0.04 0.05
① When silicon is required, the following ranges and limits are commonly specified: 0.10 %, max. 0.10 % to 0.20 %, 0.15 % to 0.35 %, 0.20 % to 0.40 %, or 0.30 % to 0.60%.
② Copper can be specified when required as 0.20 % minimum.
③ When lead is required as an added element to a standard steel, a range of 0.15 % to 0.35 % inclusive is specified. Such a steel is identified by inserting the letter L between the second and third numerals of the grade designation, for example, 10L45. A cast or heat analysis is not determinable when lead is added to the ladle stream.
④ When boron treatment for killed steels is specified, the steels can be expected to contain 0.0005 % to 0.003 % boron. If the usual titanium additive is not permitted, the steels can be expected to contain up to 0.005 % boron.
⑤ The elements bismuth, calcium, selenium, or tellurium may be added as agreed upon between purchaser and supplier.
Approximate Comparison Table Wrought Aluminum and Aluminum Alloy
China Japan United States International Organization for Standardization Germany European Standard United Kingdom
GB JIS ASTM UNS ISO Numerical Grade DIN EN/DIN W-Nr. EN BS EN/BS
1080 1080
A91080
1080 A91080 Al99.8 A91080 Al99.8 3.0285
A91080
EN-AW-Al99.8 1A
1080
A91080

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!