USA UNS G10900
AISI
American Iron and Steel Institute
1090
Corresponding Standard ASTM A29/A29M-2023
General Requirements for Steel Bars, Carbon and Alloy, Hot-Wrought
Classification Carbon Steel
Properties Good Forgability
Chemical Element Composition Content (%)
Component C Mn P S
Minimum Value 0.85 0.6 - -
Maximum Value 0.98 0.9 0.04 0.05
① When silicon is required, the following ranges and limits are commonly specified: 0.10 %, max. 0.10 % to 0.20 %, 0.15 % to 0.35 %, 0.20 % to 0.40 %, or 0.30 % to 0.60%.
② Copper can be specified when required as 0.20 % minimum.
③ When lead is required as an added element to a standard steel, a range of 0.15 % to 0.35 % inclusive is specified. Such a steel is identified by inserting the letter L between the second and third numerals of the grade designation, for example, 10L45. A cast or heat analysis is not determinable when lead is added to the ladle stream.
④ When boron treatment for killed steels is specified, the steels can be expected to contain 0.0005 % to 0.003 % boron. If the usual titanium additive is not permitted, the steels can be expected to contain up to 0.005 % boron.
⑤ The elements bismuth, calcium, selenium, or tellurium may be added as agreed upon between purchaser and supplier.
Approximate Comparison Table Wrought Aluminum and Aluminum Alloy
China Japan United States International Organization for Standardization European Standard Australia
GB JIS ASTM UNS ISO Numerical Grade EN Australian Standard AS
1090 1090
A91090
1090 A91090 Al99.9 A91090 EN-AW-Al99.9 1090
A91090