Grade W242
Corresponding Standard GJB 2664A-2018
Specification for Tungsten Base High Density Alloy for Projectile Cores
Classification Other metal materials
Density 18 ~ 18.2 g/cm3
W242 Chemical Element Composition Content (%)
Component Fe Ni More
Minimum Value 1.4 3.4 W: Remainder
Maximum Value 1.6 3.6
① Fe+Ni:4.90~5.20%
W242 Mechanical Properties
Heat Treatment or Condition
Tensile Strength
σb
Mpa
Elongation or Extension Rate
δ
%
Hardness
HBW
Sintered condition ≥833 ≥3 HRC
≥25
Heat-treated condition ≥930 ≥10 HRC
≥26