Grade 12CrMo
China ISC A30122
Corresponding Standard GB 6479-2013
Seamless Steel Tubes for High-Pressure Chemical Fertilizer Equipments
Classification Alloy Steel
12CrMo Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni Cu Mo
Minimum Value 0.08 0.17 0.4 - - 0.4 - - 0.4
Maximum Value 0.15 0.37 0.7 0.025 0.015 0.7 0.3 0.2 0.55
1 Approximate Comparison Table Structural Alloy Steel
China United States Germany France Russia Sweden United Kingdom
GB ISC ASTM/AISI DIN EN/DIN W-Nr. NF EN/NF GOST SS14 BS EN/BS
12CrMo
12CrMoV
A30122
A31122
4119 13CrMo44 1.7335 12CD4 12ХМ
12ХМФ
2216 1501-620Cr27
2 Approximate Comparison Table Structural Alloy Steel
China Japan United States International Organization for Standardization Germany France European Standard Russia Sweden United Kingdom
GB JIS ASTM ISO DIN EN/DIN NF EN/NF EN Numerical Grade GOST SS BS EN/BS
12CrMo SFVAF12 A387Gr.12
Gr.P12
F32
P32
13CrMo4-4 15CD2.05
15CD4-05
15CD4-5
13CrMo4-5 1.7335 12KHM
15KHM
2216 620
620-440
620Gr.27
3 Approximate Comparison Table Structural Alloy Steel
China Japan United States International Organization for Standardization Germany France European Standard Russia Sweden United Kingdom
GB JIS ASTM ISO DIN EN/DIN NF EN/NF EN Numerical Grade GOST SS BS EN/BS
12CrMo SCMV4 A387Gr.22
Gr.P22
F34
P34
TS34
10CrMo9-10 10CD9-10
12CD9-10
10CrMo9-10 1.7380 10KH2M 2218 622
622Gr.31
4 Approximate Comparison Table Structural Alloy Steel
China United States
GB ASTM/AISI
12CrMo A335 Grade P11
A335 Grade P12
12CrMo Corresponding Standards(Same grade name, different standards)

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!