Grade GH2132
Old Grade
Corresponding Standard YB /T 5245-1993
Hot-rolled and forged heat-resisting, superalloy bars for general force-bearing parts
Classification Special Alloy Steel
Density 7.93 g/cm3
GH2132 Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni Cu Mo Ti V B Al More
Minimum Value - - 1 - - 13.5 24 - 1 1.75 0.1 0.001 - Fe:Remainder
Maximum Value 0.08 1 2 0.02 0.02 16 27 0.25 1.5 2.3 0.5 0.01 0.4
* B, Ce added according to the calculated amount.
GH2132 Mechanical Properties
condition Heat Treatment or Condition
Tensile Strength
σb
Mpa
Elongation or Extension Rate
δ
%
Reduction of Area
ψ
%
Hardness
HBW
Test samples (room temperature)* Heat Treatment ≥931 ≥20 ≥40 HB
3.4~3.8
Sample (550°C)** Heat Treatment ≥784 ≥16 ≥28
Sample (650°C)** Heat Treatment ≥735 ≥15 ≥20
1 Approximate Comparison Table
China United States Germany France Russia United Kingdom
GB ISC Commercial Grade AISI SAE AMS DIN EN/DIN W-Nr. L-Nr. NF EN/NF GOST BS EN/BS
GH2132
(GH132)
H21320 A286 AISI660 HEV7 5525
5731
5732
5734
5737
5895
X5NiCrTi 26-15 1.4980 1.4944 Z6NCT265
ATV SMo
ЭИ 786 DTD 5026
(S/ABV)
2 Approximate Comparison Table
China Japan United States Germany European Standard United Kingdom
GB JIS Commercial Grade UNS DIN EN/DIN W-Nr. EN Numerical Grade BS EN/BS
GH2132 SUH660 A286 S66286 X6NiCrTiMoVB25-15-2 1.4980 X6NiCrTiMoVB25-15-2 1.4980 X6NiCrTiMoVB25-15-2

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!